Why Do 2 mm Homogeneous Vinyl Floors Differ in Weight and Abrasion Resistance?
Nov 16, 2026Two homogeneous PVC flooring products can both be labeled 2 mm and still feel noticeably different in the hand. Bend a strip of each product, and one may develop a pale line more readily than the other.
Two things help explain these differences: how the ingredients are proportioned and how the compound is formed into a sheet. The proportions of PVC resin, plasticizer, and mineral filler influence density and flexibility. Mixing, fusion, and pressing influence how the filler disperses and how the finished sheet forms.
PVC resin forms the continuous matrix. Heat and mixing help the PVC and plasticizer form a continuous material that holds the dispersed mineral particles. Both the amount of resin and the degree of fusion can influence how the finished product responds to bending and stretching. Research on Fillers and Fusion in Plasticized PVC
Plasticizers adjust flexibility. DOTP is one example used to make PVC more flexible. The type and amount of plasticizer also affect how the compound flows and fuses during manufacturing. Changing the formulation can therefore change the processing conditions it needs. DOTP Technical Data · Research on the Processing of Vinyl Flooring Compounds
Calcium carbonate is a common mineral filler. The amount added influences density and stiffness. Particle size, dispersion, and bonding with the PVC matrix can also affect the finished material. Formulations typically include smaller amounts of stabilizers, pigments, and processing additives to help the material withstand processing heat, develop its color, and process consistently. Research on Calcium Carbonate in Flexible PVC · Research on the PVC–Calcium Carbonate Interface
The Type I, II, and III labels on datasheets also relate to composition. ISO 10581 groups homogeneous PVC flooring by binder content by mass, which includes PVC resin, plasticizers, and stabilizers. Type I is above 55%, Type II is 35% to 55%, and Type III is 25% to below 35%. A Type I designation tells you the combined binder content exceeds 55%. Individual resin and filler proportions require separate composition data. ISO 10581:2019, Section 3.4 and Table 1
Mass per unit area equals measured thickness multiplied by average product density. At the same thickness, the denser product weighs more per square meter. Calcium carbonate has a density of about 2.7 g/cm³, compared with about 1.4 g/cm³ for PVC resin and 0.98 g/cm³ for DOTP. With comparable construction and processing, replacing some PVC resin or plasticizer with calcium carbonate generally increases the weight per square meter. Calcium Carbonate Technical Data · PVC Resin Technical Data · DOTP Technical Data
An increase in PVC resin can move weight in either direction. If the resin replaces calcium carbonate, the sheet will generally become lighter at the same thickness. If it replaces a lower-density plasticizer, the sheet may become heavier. Which ingredient it replaces determines the direction of the change.
Weight and abrasion resistance can also move independently. In one controlled study of plasticized PVC, adding calcium carbonate improved indentation resistance while increasing mass loss under the study’s abrasion conditions. A floor can resist an indentation from an equipment foot and still lose material under repeated rubbing. To compare abrasion resistance, use results for the specific products tested under the same method. Controlled Study of Fillers in Plasticized PVC
Three manufacturing steps are especially relevant: filler dispersion, PVC fusion, and sheet forming.
| Product | What the public documentation shows |
|---|---|
| Forbo Sphera | The Environmental Product Declaration (EPD) gives an average composition of about 43% PVC, 19% DOTP, and 34% calcium carbonate by finished product mass. It also describes colored granule production, controlled scattering, and steel-belt pressing. Forbo Sphera EPD, Sections 2.1 and 3.1 |
| Tarkett iQ Natural | Tarkett describes PVC made with biomass feedstock attributed through a mass-balance approach. This disclosure explains how the PVC feedstock is sourced and attributed. The actual proportions of individual materials in the finished floor require product composition data. Tarkett iQ Natural Materials Overview |
| Gerflor Mipolam Symbioz | The environmental datasheet identifies a bio-based plasticizer. This is an example of a formulation choice involving the plasticizer, a separate ingredient from the PVC resin. Gerflor Mipolam Symbioz Environmental Datasheet |
| FARFLY | FARFLY’s published range information lists PVC, calcium carbonate, and DOTP plasticizer as main ingredients. For exact ingredient proportions, forming parameters, or measured weight per square meter, refer to documentation for the specific product. FARFLY Homogeneous Vinyl Flooring Information |
Choose samples of similar measured thickness and color, cut strips of equal width, and compare them at the same room temperature. Bend each strip in the same orientation around the same rod, using the same angle and hold time. After release, look for whitening and fine cracks under the same lighting. The rod keeps the bend radius consistent and makes the comparison easier to repeat. ISO 24344 Flexibility Test
The outer side of a strip stretches during bending. Tiny voids or fine cracks can form in areas of local deformation and scatter light, leaving a pale line. Voids can also develop around filler particles when dispersion is poor or bonding to the PVC matrix is weak. Filler loading, particle characteristics, plasticizer content, degree of fusion, and the original color can all affect the visible mark. Use the result as a preliminary comparison of bending behavior. A pale line alone cannot establish calcium carbonate content. Research on Bending and Stress Whitening in PVC · Research on the PVC–Calcium Carbonate Interface
Measure the thickness at several points, then cut equal areas and weigh them on the same scale. Suppose two 10 × 10 cm samples both measure 2.0 mm thick and weigh 30.0 g and 34.0 g. Their masses per unit area are 3,000 g/m² and 3,400 g/m², respectively. If enough material is available, take several samples of each product and compare the averages. ISO 24346 Overall Thickness Measurement · ISO 23997 Mass per Unit Area
The second product weighs 400 g more per square meter and has a higher average density at the same thickness. Compaction, other fillers, and plasticizer content can all affect density. Weighing is useful for comparing samples. Composition data are needed to determine the formulation.
For a project comparison, record the bend marks, measured thickness, sample area, and weight alongside each product code. Use the corresponding technical documentation to check the material and binder information, and use the relevant test report for any performance requirement in the specification.
Add : No.5 Huaqing Intelligent Park, Huishan District, Wuxi, Jiangsu, China